studiolocreations replied to the topic Draped tealight holder in the forum General Fusing Discussion 2 years, 8 months ago
I have used little Stainless Steel 4oz sauce cups to drape tealight holders over. They work great and cost about $2 each. Find in any Kitchen store. Put on a cookie sheet, heat in your oven to about 500 degrees and apply kiln wash. This takes awhile as you need to keep reheating and applying to get a nice coat of kiln wash to stick, but I have…[Read more]