    I still haven’t found something I love all the time. I’ve had problems with both E6000 and superglue with bails pooping off pendents in heat. So I am figuring everyone thinks superglue is a bad idea as no one has mentioned it? I’ll try the fresh E6000 roughed up the glass and bail and glue both sides and heat in oven method. Ofcourse I will then have to add $5 to the cost of pendents as thats a bunch of work just to glue a bail on. ;0)~