lorin

Forum Replies Created

Viewing 4 posts - 1 through 4 (of 4 total)
  • Author
    Posts
  • #13089
    lorin
    Participant

    You  are brilliant!!! I followed your instructions, ground away the distortions and scrubbed them really clean. It is about 90% gone. I am going to order a finer grind bit as soon as I see a sale. Thank you so much!!!

    #13085
    lorin
    Participant

    Thanks! I am going to try reslumping it and using your suggestions.

    #12961
    lorin
    Participant

    I was using glassline too. It gives very poor results. So I am going to order the Kaiser paint but it doesn’t seem to offer any metalics. Perhaps I can mix a mica with a medium and use it like paint.

    Thanks for the feedback, everyone.

     

    #12917
    lorin
    Participant

    AHA! I thought I should never ever ever open the kiln until it said “completed”. The last segment didn’t end until 23 hours. A very loooong 23 hours. Thanks for the quick response!

    onward and forward.

     

Viewing 4 posts - 1 through 4 (of 4 total)