    When I just use the top elements the middle bubbles no matter how long of a soak time I have.  The kiln just seems to get too hot.  If I try to adjust by setting the temperature lower the sides don’t fuse enough.  Small pieces are ok — it’s just anything over 10″ that’s a problem.