kathymc
Forum Replies Created
- AuthorPosts
- October 26, 2012 at 10:34 pm #12725
kathymc
ParticipantThanks so much. I’m going to your web site right now!
Kathy McAlerney
October 23, 2012 at 3:04 pm #12723kathymc
ParticipantThank you Dana for your help. I am going to keep tweaking the schedule a bit. It’s almost perfect on my pendants. Still can’t get a soap dish to slump, but I will eventually! Sure appreciate your help.
Kathy McAlerney
October 21, 2012 at 1:56 pm #12721kathymc
ParticipantThanks for your help Dana. 2012-10-21
Ramp Goal temp. hold
R1 300 degrees 1150 degrees 30min.
R2 500 1475 15min.
R3 9999 1150 10 min.
R4 500 960 30min.
For Slumping a soap dish, I tried the following twice!
R1 400 1000 20min.
R2 400 1250 60min.
R3 9999 950 60min.
R4 400 100 0min.
Kathy McAlerney