jbennett replied to the topic Fusing strips on weave mold in the forum General Fusing Discussion 3 years, 4 months ago
I received a reply from Firelight with a fusing schedule. So thank you!
jbennett changed their profile picture 3 years, 4 months ago
jbennett started the topic Fusing strips on weave mold in the forum General Fusing Discussion 3 years, 4 months ago
Having a big problem (new to fusing) figuring a fusing schedule for 1/2″ System 96 single layer strips on a Firelight Forms 11″ ceramic interweave mold. I am not getting a full slump–and as I increase the temps the strips start to distort and get rounded. From the slump schedule here I see the note about the pieces being so light that they can’t…[Read more]