    I think a forum is a great idea.  I have been working with dichroic glass all summer and selling my pieces at the local Farmer’s Market.  I have done other 100 firings trying to figure out the best way to do it.  I think I’ve been making it too complicated.  I’d love to exchange ideas with people.  Annie, Lopez Island, Washington