    After the tak of flowers and islands and a moon on to the base of green field, the field shows devitrification. 🙁 I did use spray A and still got divit on the base of green but not on the many flowers. Is there any way to get rid of the divit on the green field? I cannot sift clear because I would have to fire up to 1400 and that temp would loose the definition of the components. boo hoo… any help would be greatly appreciated.