    Thanks for the suggestions.  I have been using thinfire paper, and yes many of the pieces are less than 6mm thick, expecially on the edges where I have “overhang”. from overlapping pieces.  I tried another firing using the soft fuse schedule (except that I did eliminate the steps after reaching 700 and just let the kiln cool on it’s own).  The results were much better, with only a few sharp points.  Most of these appeared to be the result of cutting rather than firing.  Should I try adding about 5 degrees or a longer hold? 