    Hello,

    hopefully you have found out by now but if not then maybe this will help out some,I don’t yet fuse any bottles but I did know someone that does a lot of it and she said that she soaked the labels and removed them  she would replace them after the fusing was done and then coat them so they were waterproof on the bottles,she made them into wine-bottle cheese boards,the skinny part was the handle she also made the utensils to go with it,hope this helps,

    Mary Gainey Free

    http://www.blueangelcat.com

    http://www.riversideartsmarket.com

     