beessg replied to the topic fusing boro in the forum Forum Help 8 years, 9 months ago
I have a friend that makes boro glass pieces and we thought we would try to make earrings out of the scraps she had laying around…we figured we would fire polish the edges, drill small holes and hang them from hoop earrings…well that didn’t work out…we couldn’t get it to work…even went up to 1500 deg F plus 30 min hold (at the 3rd…[Read more]