    I would think that you can to a degree-if you can enamel (which is glass) copper , then you should be able to fuse a thin glass layer to copper. 

     

    I have not tried, I have ony put copper into my glass.

     

    http://www.beaderydestash.etsy.com

    http://www.alexandersdesigns.com

     

    #11895
    beaderydestash
    Participant

     I have heard of people using enamel to screenprint onto glass, but I have not seen the end results for that.  They fire the enamel onto the glass too.

    #10533
    beaderydestash
    Participant

    Love that bowl!  You did a fabulous job!

     

    Jenny

    http://www.beaderydestash.etsy.com

    #11188
    beaderydestash
    Participant

    I have seen colored photos on decals and looked into the process, it is expensive so far.  But I also heard you can screen print, so i am looking into that process for myself and to resell.  Hopefully I will find it soon!

    #10596
    beaderydestash
    Participant

    Just wanted to say that I love your tree.

    Best of luck with your shop

    Jenn

    #11279
    beaderydestash
    Participant

    We use fine silver if we want to create a hanging point in our pieces.  We have done it in dichroic and regular glass fusings.  Have made bracelet links as well.  It is always pretty because it does not get firescale, just needs to be hammered prior to putting it into your piece to harden the soft metal.

    Jenny

    http://www.beaderydestash.etsy.com

    #11211
    beaderydestash
    Participant

    We make and sell our own decals for glass fusing, high fire.  You can cap over it or leave it on top we have had great success with each.  They also look great ontop of dichroic.

    http://www.beaderydestash.etsy.com

    #11186
    beaderydestash
    Participant

    I have lots to choose from at: http://www.etsy.com/shop.php?user_id=7352504

    I make them in house from clip art, photos we have taken and artwork we have drawn (even some my kids have drawn!).  We can do your photos and artwork too!

    Just visit us if interested!

    Jenny

    #11000
    beaderydestash
    Participant

    I make decals for glass fusing. I have several for sale at: http://www.beaderydestash.etsy.com

    If you have photos you would like to use, I also do custom decals.

    Just visit us if you are interested!

    Jenny

Viewing 9 posts - 1 through 9 (of 9 total)

People Who Like Thisx

Loading...