susanaart started the topic Kiln fires 200 degrees hotter than computer states in the forum Forum Help 3 years, 4 months ago
So my kiln has always fired hot. The temperature has always been offset by a fair amount. Rather than re calibrating it, I have adapted my firing schedules.
Now I am working on rather large pieces, this guess work has become a problem as I did not have a grip on the exact temperature offset. So my annealing temps are off and I have breakage.…[Read more]
susanaart replied to the topic Problem Solving Request in the forum FusedGlass.Org Website Help 3 years, 4 months ago
I use Hotline “washaway”. It’s a type of acid. Gets most of that stuff off.
FOr the dull areas: Was the glass cleaned well? Sounds like it is vitrified.susanaart changed their profile picture 3 years, 4 months ago