    The glass did not have any sign of the cracked shelf under it – no creases etc. I was using shelf paper 1/16″ under the glass and around the stainless molds. I assume it cracked on the way down because there was no healed marks on the bottom of the glass. I did discover a crack forming on the 6×6 piece but not the other one after a few days.

    I may have been aggressive taking the glass out of the the stainless dam (which I did in the kiln and on the shelf).

    The shelf was thinner than most (I got it second hand – made in taiwan with riddges on the bottom).

    #12256
    Saturations
    Participant

    1000 1000 15 min

    250 1100 15 min

    1000 1700 90 min

    9999 1500 45 min

    9999 950 180 min

    12 800 15 min

    24 700 10 min

    120 100 0 min

     