Mary Kay Nitchie replied to the topic bullseye opal not fusing in the forum General Fusing Discussion 3 years, 3 months ago
Hi Jojo,
I think that your opal glass needed either more time or a higher temperature. The fiber paper turns brown as the binders are burning out. These binders are burned up and the paper turns white again at the process temperature for the glass.