mariafromcali
mariafromcali changed their profile picture 2 years, 5 months ago
mariafromcali changed their profile picture 2 years, 5 months ago
mariafromcali replied to the topic Fusing schedule to just soften edges after sawing in the forum Glass Fusing 2 years, 5 months ago
I wanted to give a shout out to everyone who suggested the soft fusing schedule here at FusedGlass.org. It was PERFECT. I am so happy with my last run.
mariafromcali replied to the topic Kiln and glass supplies in Eugene, OR in the forum Stuff for Sale 2 years, 6 months ago
Why aren’t you closer to me? I live in CA
mariafromcali replied to the topic Fusing schedule to just soften edges after sawing in the forum Glass Fusing 2 years, 6 months ago
Thank you so much djjohnese! I do keep a log of each run I make. It really helps figure out what went wrong or right. I really appreciate your insight and help. I will post some pics after my next run. thanks again.
mariafromcali replied to the topic Fusing schedule to just soften edges after sawing in the forum Glass Fusing 2 years, 7 months ago
Thank you LaurieMae! Sounds like just what I need. Much appreciated!
mariafromcali started the topic Fusing schedule to just soften edges after sawing in the forum Glass Fusing 2 years, 7 months ago
Hi all,
Fairly new to glass fusing. I would like to find a firing schedule that just softens/rounds the edges of an already fired one layer + frit glass. Here is what I have done: Started with a thin sheet of french vanilla, added frit on top, full fused. Then cut up into small shapes (squares, rectangles) for jewelry. Now I just want to fire to…[Read more]mariafromcali became a registered member 2 years, 7 months ago