Lynn g replied to the topic Cleaning Fine silver wire after firing in the forum General Fusing Discussion 11 years, 3 months ago
Wire-brush or use wet-dry sandpaper to remove the oxide. You can then tumble it with stainless steel shot to polish and work-harden it.