IMG_20190716_182948238
img_20190716_182948238

Kiln Pressed glass 😎. I'm new to fusing glass and this is my first time doing this. I just love the results. I had several problems along the way but I didn't give up. It took 6 firings, a tile saw, grinder and lots of love. Hope you like it 😊.
Leave a comment if you have any suggestions. 🤔
Thanks