Edpal247 replied to the topic Vent Kiln During Cooling in the forum General Fusing Discussion 3 years, 9 months ago
On thick pieces(1″/25mm+)in a thick mold or dam setup the kiln temp can be quite deceiving compared to the glass temp. I’ve pulled out thick glass blanks when the kiln read 75-80f, wrapped them in a thermal blanket and then shot them with the infra-red thermometer 10-15 minutes later. Close to 150f. 3-6mm flatwork on a ceramic fiber shelf your…[Read more]