ParticipantThanks Barry,
This site is so helpful! You all are so willing to share your experiences and knowledge!
CarenJanuary 25, 2010 at 11:52 pm #11484Caren Johnson
ParticipantThis is an interesting subject because I have been firing some rather large pieces, and they break if cooled too quickly. I am having a hard time deciding how to cool them more slowly withoug risking devitirfication as well. And in your experience, fusers, would the devitification spray prevent both these occurrences? Thanks, Caren
November 17, 2009 at 3:01 am #11427Caren Johnson
ParticipantI have ordered dichro from ebay and it has been very nice. You can always ask about where it came from. Also have ordered from well known name suppliers and got bags of scrap that had little usable glass; all with soft ends and little variety and much of it very scratched on the surface.
November 17, 2009 at 2:57 am #11041Caren Johnson
ParticipantHey guys, I am not a novice fuser, but I am brand new to this web site (less than 10 minutes), and already I’m loving it! Lots and lots of helpful information.