BonnieJean replied to the topic Draped tealight holder in the forum General Fusing Discussion 1 year, 1 month ago
did you put thin fire under the glass? You need to put a piece of thinfire shelf paper over your mold,and center the glass over that. That will keeps the glass from sticking to the mold, or post in this case. It also gives you the texture in your drape.