bigtexun
bigtexun replied to the topic Devitrification, any fix after the fact? in the forum General Fusing Discussion 3 months, 3 weeks ago
I use whatever cold-work tooling that is appropriate, if the pieces are large enough to handle. So far I have a pneumatic wet grinder, and I also use emery paper from home depot, as well as a regular dry belt sander. A sand blaster and a wet belt grinder is on my Christmas list for NEXT year (this year I bought a house with a detached studio for…[Read more]
bigtexun replied to the topic slab layer firing in the forum General Fusing Discussion 2 years, 9 months ago
Paul’s chart is for annealing only. You aren’t going to be fusing or firepolishing at the annealing temperatures. I think Paul misunderstood the information you were looking for.
Go to the bullseye site and find the chart named “Basic Firing Schedules for Bullseye Glass 2020”. If you look there you will see the tac-fuse/fire-polish is around…[Read more]
bigtexun changed their profile picture 2 years, 9 months ago
bigtexun became a registered member 2 years, 9 months ago