I just purchased the Zephyr ring saw and was anxious to begin cutting pieces for a new project. However, when attempting to cut the glass, it chips. I’m trying to let the blade do the work but it doesn’t seem to help. Has anyone else had issues with this or know what I’m doing that is causing this?
I have used one of these for a few years, and have had no real problems with it, other than I get pretty damp from the water. I make sure there is lots of water in the reservoir. It helps to not force the saw too hard.