Home › Forums › Glass Fusing › General Fusing Discussion › Wire for hangers
Can I use any kind of wire fused between glass layers for a hanger? Is there any specific wire recommended?
Thanks,
Annie
Use copper or silver. Those 2 metals are fusible with glass. There may be others (platinum comes to mind, but not sure)
Both pretty easy to find, and not too expensive
You can find nickle chromium high temp wire at most glass supply places; i.e.,
http://www.delphiglass.com/fusing-supplies/fusing-tools/17-gauge-high-temp-wire
Dana W.
Jester’s Baubles Fused Glass Designs
http://www.jestersbaubles.com