Hi I am new to fusing having recently done a beginners course now wanting to purchase a kiln but needs to be easy to use and with pre programmed schedules. I’m thinking shuttle firebox ?? All advice welcome
I would avoid preprogrammed schedules. If you want to fuse glass you should lean how to choose / change firing schedules to meet your needs. There is a good tutorial on this site.