I want to start the projects in the Scrap Glass ebook but am concerned about the scraps being clean enough after being handled on previous projects. Is this an issue when using scraps?
jAn easy way to clean scrap glass is to put it in a plastic bin, add water and a little soap, then swirl it all around with a cheap paintbrush. Rinse well.