Can I slump a tack-fused piece, or will it ruin the shapes?
Is perfectly possible if you stay in the 630C to 670C range
Stephen Richard
blogs at: http://www.verrier-glass.blogspot.com/ and http://www.glasstips.blogspot.com/
Thank you, Stephen. It worked perfectly.