    JanneR
    Participant

    Can I do it? How would I adjust my firing formula? I’m not trying to get a gloss but an overall satin finish on coldworked pieces.

    #13307
    wordana
    Participant

    If you coldwork your pieces down to a 400 grit finish, it will polish out with slumping temps (kind of in between a matte and a full gloss. Works best on edges — it’s hard to get all the scratches out on a flat piece unless you are coldworking with a sandblaster!).

    Dana W.

    Jester’s Baubles Fused Glass Designs

    http://www.jestersbaubles.com