Slumping a deviled egg dish (12)

Home Forums Glass Fusing General Fusing Discussion Slumping a deviled egg dish (12)

Viewing 2 posts - 1 through 2 (of 2 total)
  • Author
    Posts
  • #10123
    suzylmoore
    Participant

    I have tried to slump an deviled egg dish. Without success. ¬†Dish is 12×12 with twelve indents. I am using 6mm of fused glass. Any suggestions?

     

    #13308
    wordana
    Participant

    Without a firing schedule we can’t even begin to guess, but in general, you are going to need a relatively long hold to get those small indentions to slump completely.

    Dana W.

    Jester’s Baubles Fused Glass Designs

    http://www.jestersbaubles.com