Hi, I have a SC3 Paragon Kiln which is in Celsius & was hoping someone might have some Ramp…, Temperatures… & hold time schedules for slumping or melting a glass beer bottle… any help would be apprecated…. Cheers Jenny..
Hi Jenny – sorry for the long delayed response. Your post was in the forum help section (intended for help on using this website) so I never saw it.
I use the “Soft Fuse/3 layer” schedule on this site to slump bottles with consistent success. Just click “Firing Schedules” under the tools menu above.