I am relatively new to glass fusing, I created a project which I really love, but there is one item on the piece that does not look right. Is there any way to remove something once it has been tack fused to a piece? There are several fish tack fused to a background piece of glass. One of the fish looks weird and the piece would be so beautiful if I could somehow get it off and replace it with another. Is this even remotely possible?
But it is possible with a lot of work. You have to abrade the unwanted pieces from the surface of the piece. I have sandblasted off something that I absolutly had to save.
Mainly, it it just isn’t worth the effort, especially on a delicate tack fused piece. Make another is my recommendation.