I’m interested in experimenting with recycled glass and I’ve seen the rings or circles that can be made using wine/beer bottles – does anyone know a good firing schedule to achieve this effect?
I have a lot of stained glass sheets and I use them to slump pieces or to try out new molds.
I use the same slumping schedule as a regular slump but I lowered it by 40 degrees and only hold for half of my regular slump. It tool some trial and error but it seems to work. I am going to try some on the big Skutt and see how they tuen out, I will post after so that you can see,