I have purchased Paul’s book on What to do with scrap glass and I have made several things from it. But I Have a box full of projects that have not worked out quite as planned. Can I use this glass for those projects in the book?
I use old projects for pot melts and pulling cane. Some glass can shift coe after several fusing so thats the only thing i can think of that could be a problem.