    I have a HP Laser Jet 2035 which was recommended for printing my decals but I cannot get them to print off clearly. The decal is always smudged. It is like the printer is pushing them through too fast. I hand feed one sheet at a time and I am using the proper paper. If anyone else has had this problem I would love to hear from you.

    #13338
    nella
    Participant

    Hi,,r u warming up your printer,,,I have been told to run BLANK sheets of paper,,maybe 6 or so and warm up the printer BEFORE you run your decal paper,,hope this helps

    nella

     

     

     

    #13339
    glasshive
    Participant

    Always warm it up but doesnt seem to help so far.

    #13340
    nella
    Participant

    sorry,,thats all I “got”:)…I just let mine dry for awhile before I touch it or put it in the water,,and I also use distilled water,,maybe someone else knows more…good luck