    I purchased a pot melt stand and bowl.  Tried my 1st pot melt and it left glass in the bottom of the pot. It set in the corner for months until this weekend.  While I was doing a drop ring vase I set up a mold to catch the glass from the pot melt, place 2 kiln post on the sides of the mold and turned the pot melt bowl upside down and placed on the kiln posts.  After my drop ring vase was completed I lifted the pot melt bowl and all the glass from inside the bowl was gone and collected in the bottom mold.  Just thought I would share my successfull expertiment.Smile