When I fire my project one side is rough and I don’t know how to polish it so it is as smooth as the other side. Please help. Thanks, Kathy
In kiln formed glass the bottom will always be as rough as what it comes into contact with – shelf, mould, etc. So you have to make the separator as smooth as possible.
Stephen Richard
blogs at: http://www.verrier-glass.blogspot.com/ and http://www.glasstips.blogspot.com/
Thanks so much. That was what I was afraid of. I will be more diligent in my kiln wash application. Kathy