Hi,
I’ve seen so much about this but no real explanations of what it is. What is Photopolymer Masking and how do you do it?
Thanks,
dee
This is a process that uses a photographic process to mask dichroic glass. The glass is etched with Armour Etch yielding the desired design.
We teach a course on this and sell the materials.
Barry Kaiser
Web Site http://www.kaiserglass.com