- September 6, 2008 at 10:41 pm #9198
jana456
ParticipantI purchased and have tried to use photo decals, but when I fire, there is nothing there. I have red the instructions repeatedly. Is there a secret?
September 7, 2008 at 4:00 am #10724groovyglassgirl
ParticipantYes, the secret is the ink that you print with. Are you using a laser printer?
September 7, 2008 at 4:55 am #10725glassartguy
ParticipantNot only do you need to print with a laser printer, it has to use carbon toner. Evidently some use a polymer that would just burn off.
For anyone who lives around Portland, Oregon. In October Bullseye is having a free class on transfering images onto glass.
Glassartman
September 7, 2008 at 7:06 am #10726cerebus
ParticipantHere’s are two links I found when I was considering doing photo realistic decals. It sounds like you need special "ceramic toners" in an inkjet printer for color, or a toner with a high iron oxide content in a laser printer, to get it to work. Hope this helps.
Cerebus
http://www.glass-fusing-made-easy.com/fusing-photo-paper.html
http://www.dcphub.com/Process.htm
“You use a glass mirror to see your face; you use works of art to see your soul” -George Bernard Shaw
September 7, 2008 at 8:46 am #10727jana456
ParticipantPerfect! THanks so much for the info!
- AuthorPosts
Viewing 5 posts - 1 through 5 (of 5 total)
- You must be logged in to reply to this topic.