    Our newest eBook is out! Take a look at FusedGlassBooks.com

    Loads of projects, over 120 color photos and illustrations. Just $15.

    #12875
    CH Art Glass
    Participant

    Your new book is wonderful.  I’m working on a project using the techniques as we speak.  One question: Why do you recommend fiber paper under shelf paper in your projects?

    #12876
    Anonymous
    Inactive

    It allows air to escape and guarantees no bubbles between the shelf and glass.