Does anyone have a Moretti firing schedule. or can tell me how to modify a 90 COE one?
It’s 104 COE, when they don’t work out so well it’s an expensive failure. I’d like to have more consistant results with a 104 schedule. Thanks
Moretti/Effetre – nominal CoE 104
Strain point 448C
Annealing range 493-498C
Softening Point 565C
You can use these figures to modify a Bullseye, S96 or Uroboros schedule.