What advice does anyone have for draping luminescent glass on a stainless cylinder? I would like the luminescence to be on the outside of the vase. Is this advisable? I did a fire polish luminescent-side down on Bullseye thinfire first. Recommendations? I really appreciate the Forum as I’ve only been fusing since last year! Thank you. Dianne M.