I’ve had a look on the search facility and online but I cannot find much info on how to do something in particular. I want to make little glass balls for embellishing fused glass pendants/tiles/panels etc…and can’t find how it’s done.
I expect that the balls start off as little squares of bullseye and then put them in a hot kiln so that they draw up. What temperature should I use? What sort of programme and timing? I expect I could vent immediately as they won’t really shock?
Thank you in advance
January 8, 2012 at 10:46 pm #12375chookie
ParticipantThe hunt is over after I was looking through the projects above, the fold over bailed pendants have the info I was looing for on. Just like the ‘A’ Team, I love it when a plan comes together
January 9, 2012 at 4:36 pm #12376Becki
ParticipantYou can also lay course frit out on the shelf, separate it and fire to full fuse. You’ll get nice little solid color frit balls!
January 9, 2012 at 8:39 pm #12377bookie13
ParticipantI just use a torch and a charcoal block. works like a charm.
Heat it in the torch. Balls up beautifully.
Barry Kaiser
Web Site http://www.kaiserglass.com
Glass Classes: http://www.Kaiserglass.com/classes.html
January 9, 2012 at 11:07 pm #12378chookie
ParticipantThank you Mr Kaiser, helpful as per usual
January 9, 2012 at 11:08 pm #12379chookie
ParticipantThat’s sounds like fun, I shall have a go at that too!
August 11, 2018 at 5:54 am #12380VictoriaBryant
ParticipantI was with little glass balls in my childhood playing with them is my favorite task I was play the whole day and did not do my college work. I want some writing service that was clear from any scam because I hear about smartwritingservice.com scam although it was clear later but we are worried about that.
August 18, 2018 at 9:47 am #12381lizabajaj
ParticipantThanks for the nice blog. It was very useful for me. I’m happy I found this blog. Thank you for sharing with us,I too always learn something new from your post.
Escorts in Dubai Dubai Escorts Escorts in Dubai Escorts in Dubai Dubai Escorts Dubai Escorts
- AuthorPosts
- You must be logged in to reply to this topic.