I have been making initial jewlery with dichroic glass. I am doing etching. I put on a decal for the ititial then do etching. I feel like I am wasting good dichroic though. The only thing left of the dichroic is the actual letter. Any ideas to help do the reverse? Maybe decals that are letters that I can fire? Where to get them?
You can buy some dichroic paper and paper punches. I have used the paper with butterfly and dragonfly puches and fused it to my glass. They turn out very nice.