How can I create an organic, slightly wavy, irregular edge on my shallow bowls?
Try varying thickness along the edge. 1/4″ will stay put, but 1/8″ will draw in (because glass wants to be 1/4″).
In the same way, put some beads along the border.
Yes! Thank you. That will do it.
Cut the glass with a wave form in the edge.