I need to rapid fire a black and white decal onto my glass and I don’t know how to create my firing schedule. It’s 1/8 of an inch thick. I have a paragon kiln with sentry 3 controller. I’m new at programming kiln any help would be appreciated. I was told it was cone 22 but have no idea how to implement that. I’m suppose to fire at 1100.
Sorry I can’t help but would also be interested in your answers. I also have a Paragon with Speed Firing, I can’t find any information about them or what they are suitable for! I have my own programmed firings, trial and error, that work for me but am curious about the speed settings and what I can use them for.