Hair spray?
Home › Forums › Glass Fusing › General Fusing Discussion › Hair spray?
- This topic has 7 replies, 6 voices, and was last updated 6 years, 1 month ago by
wordana.
- AuthorPosts
- March 17, 2016 at 1:55 pm #10325
Mothsgal
ParticipantI’m still learning about this wonderful world of fused glass that I’ve fallen in love with. I was perusing the tutorials and was curious about the use of hair spray (used in the fossil vitra tutorial to adhere frit to leaves). Can it be used glass on glass? I like to use frit to add subtle shading across the glass. can I use hairspray to get the frit to stick to the glass?
Thanks!!!
March 18, 2016 at 12:42 pm #13589RubyCruiser
ParticipantYes, you can. I’ve been using it for a while and haven’t had an issue with it.
March 18, 2016 at 3:28 pm #13590Mothsgal
ParticipantThank you!!
March 19, 2016 at 3:54 pm #13591MA
ParticipantMA
I have used hairspray also and find it works very well for powder applications and mica, too.
March 27, 2016 at 12:07 am #13592gypsycolleen
ParticipantThis is great information to have!
What type is best to use? Pump? Aerosol? Brand?
Thank you!
March 28, 2016 at 7:51 pm #13593aknight
ParticipantI use the cheapest hairspray and it works fine. Amy
April 6, 2016 at 6:33 pm #13594wordana
ParticipantCheap — White Rain or Sauve in the bottle. I would suggest NOT spraying it on, but using an eyedropper.
Dana W,
Jester’s Baubles Fused Glass Designs
jestersbaubles.blogspot.com
April 6, 2016 at 6:33 pm #13595wordana
ParticipantCheap — White Rain or Sauve in the bottle. I would suggest NOT spraying it on, but using an eyedropper.
Dana W,
Jester’s Baubles Fused Glass Designs
jestersbaubles.blogspot.com