Home › Forums › Glass Fusing › General Fusing Discussion › Gold Fire Pens
I recently bought a gold fire pen to add accents to my dichroic jewelry. does anyone have a fusing schedule for them. I’m assuming I need to vent the kiln to 1000 degrees, but not sure how high I should go with the temp. Any thoughts?
Lori
I’ve fired these similar to firing the gold decals. With the pen delphi offers, they recommend firing to about 1150. I think I’ve fired them higher.
Dana W.
Thanks Dana, I will give it a try!