    So the kiln had a melt down and ruined a large shelf.  Any possible way to remove that glass that is imbedded and use the other side…. help???

     

    #12636
    Anonymous
    Inactive

    Sandblast.

    You can also probably just scrape off what you can and flip the shelf over. So long as the glass on the bottom side doesn’t touch anything it won’t be a problem.



    Paul
    FusedGlass.Org