I’m pretty new to all this. Yesterday I tried fusing my first spoons, and for the first time I set the firing schedule from the instructions (versus using a preset schedule). The spoons seemed to fire way too hot so either I entered the schedule wrong (I was very careful when I entered it) or my kiln runs hot. Today I am trying a frit slurry but I’m hesitant to try entering the firing schedule provided in the instructions. My question is…to do a fuse and slump all at once will it be safe to use one of the preset schedules and would I use the slump or full fuse schedule? Thanks!