Home › Forums › Glass Fusing › General Fusing Discussion › fusing schedule for adhesion
I am looking for some advice or a fusing schedule to attach an upright wavy piece to a glass base- the upright is 10″ long by 4″ high.
Everytime I try, it melts down….
Thanks.